| Kaou KO-95 Cobalt Stearate |
| Standard |
Standard of Dunlop |
| Appearance |
blue violet or red purple granular |
| Quality index |
Item |
Index |
Mass percent of Cobalt |
9.6±0.6 % |
Softening point |
80~100 ℃ |
Ash |
≤ 13.4 % |
Loss on heat (105℃) |
≤2.0 % |
Density |
1.09±0.03 g/cm3 |
Infrared spectrum (compared with the standard spectra) |
comparable |
|
| Uses |
This product can be used for manufacturing steel radial tires , and also for steel wire reinforced rubber conveyor belts,steel wire braided tuber hoses and other rubber products with metal reinforcements |
| Packing |
Net wt 25Kg, packed in double-layer sealed plastic bag, with cardboard drum outside ( or following your demands) |
| Storage |
one year in cool and ventilating place, avoid direct sunlight |
| Picture |
 |
|
|
|
|